COLOUR FREE LEAD CD20 ORANGE
Orange- CD20
Without lead
Firing temperature: 980-1280°C
Formula: Cd-S-Se-Zr-Si
COLORED WHITE ENGOBE CC01
Engobes range.
Possibility to mix them together.
Usable on raw pieces or bisquewares, for soaking or decoration.
Temperature of firing : 940-1000°C
Free of lead
STRONTIUM CARBONATE
Ref : CARSTR
Molar formula
CO3Sr2
Molar mass: 148
BARIUM CARBONATE
CARBAR
Molar formula:
CO2Ba
Molar mass: 197
Alumina ball's diam 18mm
Milling ball
Alumina 92%
Bar for 1400°C maximum L 150x4 mm - 4000001500
Lustre platine ( Ex E-11050/38)
GROUPE III
Firing temperature: 850-990°C
Satin transparent glaze - 5888
Without lead.
For enamelling ceramic pieces in red or white clay.La température de cuisson conseillée est de 980°C.
The recommended firing temperature is 980°C.
Transparent Sèvres blue enamel - 5517
For enamelling white majolica.
Recommended firing temperature between 1000-1050°C.
Open cutter small model diameter 6 mm - 530
Half Round Hole Cutter
Transparent glaze - 5005
Composed of Fritte.
Glossy transparent enamel is widely used for enamelling white majolica, for its excellent transparency, shine and color development.
It can be used for culinary ceramics because it does not give lead solubility under usual working conditions.
Can be decorated both under and on enamel.
It is specially indicated for obtaining coloured enamels.
The firing temperature varies between 980-1050ºC.
Alkaline base for crystallization - 3110 (FR 5)
Alkaline lead-free enamel with high temperature range.
Composed of frit.
Used in the production of crystallizations at high temperature.
Temperature range 1000-1300°C.
Sponge half drop of water on wooden handle - 225HM001
ø 50 mm
L. 110 mm
GLAZE FOR STONEWARE AND PORCELAIN 010586 PINK SALMON JASPE
Pink salmon jaspé 0-10586
GROUPE I
Firing temperature: 1250-1300°C
Pinky brown 010285 Mat
Matte (or matt) surface in glaze(glaze is NOT shiny, matte is the opposite of glossy)
Glazes for stonewares and porcelains
ENGOBE LIQUID ENSPCC01L WHITE EXTRA 250GR
Extra white ENSPCC01LL
Without lead Groupe 1
250gr
Firing temperature: 980°C-1050°C
LIQUID GLAZE EOSP21L PINK OPAQUE WITHOUT LEAD 250GR
PINK - EOSP21 L
GROUPE I whithout Lead
Firing temperature: 980°C
250gr
ENGOBE LIQUIDE ENSP11L TURQUOISE 250GR
Turquoise ENSP11L
Engobe liquide prêt à l'emploi
Conditionnement : 250GR
Groupe I
Cuisson 980°C-1050°C
ORANGE FLECKED YELLOW OPAC LIQUID GLAZE PSE22
Orange flecked yellow PSE22
Yellow natural modeling clay firing salmon - MJAUNE5
For initiation in clay. Adapted for modelling, stamping and throwing.
It dries in 3-4 days around with room temperature conditions.
CAUTION : realisations may crumble if you do not fire.
Firing temperature : 980-1000°C (1796-1832°F)
It can not be glazed.
ENGOBE POWDER ENSP00 BLANC
White ENSP00 underglaze
GI Without lead
ENAMEL XP3059 DUCK BLUE OPAQUE LEAD-FREE
Duck blue
Ref : XP3059
Group I lead free
Cooking range : 980-1020°C
Bright red XP3052/T
Free of lead
GROUPE I
Temperature of firing : 930-1050°C
Coefficient of expansion
ENAMEL XP3050 BRIGHT ORANGE YELLOW OPAQUE LEAD FREE
Glaze Copper green XP3048
Groupe I
Firing temparature: 960-1050°C
Sculpture loop toll in stainless steel for clay L. 20 cm - WMT1008