Sponge half drop of water on wooden handle - 225HM001
ø 50 mm
L. 110 mm
SPONGE WITH CYLINDRICAL WOODEN HANDLE ROUND TIP DIAM 16 MM L 80 MM
Sponge on cylindrical wooden handle - 101HM001
GLAZE FOR STONEWARE AND PORCELAIN 010586 PINK SALMON JASPE
Pink salmon jaspé 0-10586
GROUPE I
Firing temperature: 1250-1300°C
Red cherry jaspé 010575
GROUPE I
Firing temperature: 1250-1300°C
Pinky brown 010285 Mat
Matte (or matt) surface in glaze(glaze is NOT shiny, matte is the opposite of glossy)
Glazes for stonewares and porcelains
ENGOBE LIQUID ENSPCC01L WHITE EXTRA 250GR
Extra white ENSPCC01LL
Without lead Groupe 1
250gr
Firing temperature: 980°C-1050°C
LIQUID GLAZE EOSP21L PINK OPAQUE WITHOUT LEAD 250GR
PINK - EOSP21 L
GROUPE I whithout Lead
Firing temperature: 980°C
250gr
LIQUID ENGOBE ENSP16L CARAMEL 250GR
Caramel ENSP16L
Without lead Groupe 1
250GR
ENGOBE LIQUIDE ENSP11L TURQUOISE 250GR
Turquoise ENSP11L
Engobe liquide prêt à l'emploi
Conditionnement : 250GR
Groupe I
Cuisson 980°C-1050°C
UNDERGLAZE LIQUID ENSP17L BLUE COBALT 250GR
Cobalt blue ENSP17L Underglaze liquid
GI without lead
250GR
ORANGE FLECKED YELLOW OPAC LIQUID GLAZE PSE22
Orange flecked yellow PSE22
Yellow natural modeling clay firing salmon - MJAUNE5
For initiation in clay. Adapted for modelling, stamping and throwing.
It dries in 3-4 days around with room temperature conditions.
CAUTION : realisations may crumble if you do not fire.
Firing temperature : 980-1000°C (1796-1832°F)
It can not be glazed.